Aluminium casting master alloy to adject the alloy content Ti / Mn / Fe / Cu / Cr additive

$800.00 - $1,000.00
Min. Order
1 Ton
GET LATEST PRICE ON APP
Choose your specifications
Company Information

Henan Adtech Metallurgical Materials Co., Ltd.

CN Manufacturer, Trading Company
Response Time
<24h
Response Rate:
100%
Transactions
---
7 Years Paid Supplier Gold Supplier Onsite Check
Learn More

Quick Details

Port: master alloy : any China port
Payment Terms: L/C,T/T,Western Union,MoneyGram
Supply Ability: 2000 Metric Ton/Metric Tons per Month
Place of Origin: Henan China
Brand Name: AdTech
Model Number: AL-Sr10
Application: aluminum alloy casting
Shape: Powder
Material: Strontium Powder
Chemical Composition: Al- Sr10%
Model: AL-Sr10
Unit Weight: 100-500g
Applicable Temperature: 700℃-740℃
Sample: free sample for 2 pies
Ship time: 7-15 days
Product name: Aluminum master alloy casting additive
Purity: 99.8%+
Size: Clints Requiry
Color: silver package
Usage: Metallurgy casting
Packaging Detail: master alloy : 2KG/Bag, 40KG/carton, 1000KG/Dozen

Aluminium casting master alloy to adject the alloy content  Ti / Mn / Fe / Cu / Cr additive 

 

1. Excellent texture structure 

2. Improve mechanical performance

3. Lasting remelting modification 

4. Accurate and clean addition

5.Save the inventory,transport and storage costs

6.Usage : changing crystal lattice of aluminum and aluminum alloy.

 

Method of application 

As to aluminum strontium alloy, remove package and keep the temperature at 730-745°C after alloying, then keep in stove for 10 mins, and fully mix , refine for another 10 mins with high-purity nitrogen or argon gas, finallly keep in stove for 25 and done.

 

Component analysis

Al-Sr.jpg

 8

 

Package and Conserve 

2KG/Bag, 40KG/carton, 1000KG/Dozen,

keep  in ventilated and dry environment.

Guarantee period : 12 moths.

Gather package and dispose, no burning inside stove.

 

 1.jpg

 

User's Guide

1. Dosage:To add according to the customer different Content request . AL-Sr10 normal add

    dosage to per Ton molten aluminum is in 0.2 ~0.4%

 

2.Add time: Add AL - Sr10 when aluminum liquid temperature is in 730-740 ℃ after all materials          added and finished refining, and rest 5 minutes. Then stir with high purity Nitrogen for 10~15              minutes, then rest for 20 ~25 minutes to casting.

 

Methods for analysis
Atomic absorption method or the ICP analysis of United States; This product does not apply to spectroscopic analysis.

 